ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel

Category Metal , Ferrous Metal , Alloy Steel , AISI 9000 Series Steel , Low Alloy Steel , Carbon Steel , Low Carbon Steel
Manufacturer ATI Allvac
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 9310 UNS G93106, UNS H93100 Specialty Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: Automotive applications, structural components, gears, rods, heat-treatable shafts.Property values are for samples in the metallurgical condition: 1630°F normalized.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 27
27
Tensile Strength, Ultimate 907 MPa
132000 psi
Tensile Strength, Yield 571 MPa

@Strain 0.200 %
82800 psi

@Strain 0.200 %
Elongation at Break 19 %
19 %
Reduction of Area 58 %
58 %
Component Elements Properties Metric English Comments
Carbon, C 0.10 %
0.10 %
Chromium, Cr 1.2 %
1.2 %
Iron, Fe 94 %
94 %
as balance
Manganese, Mn 0.55 %
0.55 %
Molybdenum, Mo 0.12 %
0.12 %
Nickel, Ni 3.33 %
3.33 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.25 %
0.25 %
Sulfur, S 0.010 %
0.010 %