Uses: Process equipment, flue-gas scrubber systems, multi-effect evaporators for brines, seawater, pulp & paper liquors.Property values are for samples in the metallurgical condition: 2050°F anneal.Information provided by Allvac, An Allegheny Teledyne Company.
Physical Properties Metric English Comments
Density 8.06 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 90
90
Tensile Strength, Ultimate 760 MPa
110000 psi
Tensile Strength, Yield 345 MPa

@Strain 0.200 %
50000 psi

@Strain 0.200 %
Elongation at Break 45 %
45 %
Reduction of Area 60 %
60 %
Component Elements Properties Metric English Comments
Carbon, C 0.015 %
0.015 %
Chromium, Cr 21 %
21 %
Iron, Fe 46 %
46 %
as balance
Manganese, Mn 1.0 %
1.0 %
Molybdenum, Mo 6.5 %
6.5 %
Nickel, Ni 24.5 %
24.5 %
Nitrogen, N 0.22 %
0.22 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.015 %
0.015 %