ATI Allvac® Nickelvac® W-722 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer ATI Allvac
Trade Name Nickelvac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® Nickelvac® W-722 Nickel Superalloy, Heat Treatment: 982°C (1800°F) + Age.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Ring components in jet engines.
Physical Properties Metric English Comments
Density 8.24 g/cc
0.298 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 318
318
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 346
346
Estimated from Rockwell C value.
Hardness, Rockwell C 34
34
Hardness, Vickers 333
333
Estimated from Rockwell C value.
Tensile Strength, Ultimate 1172 MPa
170000 psi
Tensile Strength, Yield 759 MPa

@Strain 0.200 %
110000 psi

@Strain 0.200 %
Elongation at Break 20 %
20 %
Reduction of Area 25 %
25 %
Component Elements Properties Metric English Comments
Aluminum, Al 0.70 %
0.70 %
Carbon, C 0.040 %
0.040 %
Chromium, Cr 15.5 %
15.5 %
Iron, Fe 7.0 %
7.0 %
Nickel, Ni >= 70 %
>= 70 %
as balance
Titanium, Ti 2.4 %
2.4 %