Material Notes:
Aartel 800AM is a new antimicrobial grade that offers the same excellent physical and mechanical properties of standard Aartel grades plus the added benefit of protection against microbial growth, providing a competitive advantage for products in the most challenging environments.Information provided by Gehrig & Associates
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ISO 1183
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.026 cm/cm
0.026 in/in
ISO 294-4
Melt Flow 11.28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
11.28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.0 MPa
8410 psi
(50mm/min); ISO 527-2/1A
Elongation at Yield 11 %
11 %
(50mm/min); ISO 527-2/1A
Tensile Modulus 2.50 GPa
363 ksi
(1mm/min); ISO 527-2/1A
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1e
Thermal Properties Metric English Comments
Melting Point 167 °C
333 °F
(10°C/min); ISO 11357-1,2,3
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2