Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 66.2 MPa
9600 psi
ASTM D638
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
350 °F
ASTM D648