Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AVPP C 200-2 MELT 30 Clarified Virgin Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Aaron Industries Corporation
Trade Name AVPP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AVPP C 200-2 MELT 30 Clarified Virgin Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A natural polypropylene copolymer resin specifically designed for injection molding applications - containing clarifiers.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Linear Mold Shrinkage 0.022 cm/cm
0.022 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved