Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 50-3/AboCure 50-17 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-3/AboCure 50-17 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months.
Physical Properties Metric English Comments
Viscosity 11000 - 14000 cP
11000 - 14000 cP
50-3
110 cP

@Temperature 70.0 °C
110 cP

@Temperature 158 °F
at 100/26 (50-3/50-17) pbw
Mechanical Properties Metric English Comments
Hardness, Rockwell M 106
106
Tensile Strength, Ultimate 65.84 MPa
9549 psi
Elongation at Break 4.4 %
4.4 %
Flexural Yield Strength 93.1 MPa
13500 psi
Flexural Modulus 2.69 GPa
390 ksi
Compressive Yield Strength 115.83 MPa
16800 psi
Compressive Modulus 2.59 GPa
375 ksi
Izod Impact, Notched 0.310 J/cm
0.581 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 1.22e+16 ohm-cm
1.22e+16 ohm-cm
Surface Resistance >= 7.85e+15 ohm
>= 7.85e+15 ohm
Dielectric Constant 3.56

@Frequency 1e+6 Hz
3.56

@Frequency 1e+6 Hz
4.06

@Frequency 1000 Hz
4.06

@Frequency 1000 Hz
4.1

@Frequency 60 Hz
4.1

@Frequency 60 Hz
Dissipation Factor 0.0054

@Frequency 60 Hz
0.0054

@Frequency 60 Hz
0.015

@Frequency 1000 Hz
0.015

@Frequency 1000 Hz
0.036

@Frequency 1e+6 Hz
0.036

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 68.0 min

@Temperature 70.0 °C
68.0 min

@Temperature 158 °F
500 g
Descriptive Properties Value Comments
Exotherm 238°C
Peak
Users viewing this material also viewed the following: