Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: FastBest rigid, chemical, and heat properties with room temperature cureMain Drawbacks: Too fast for thick castings (>1inch)Needs precise ratiosProcessing: 100/5 ratio. Room temperature cure 2 to 8 hours, optional post-cure 2 to 4 hours at 80 to 120°C.Information provided by Abatron.
Physical Properties Metric English Comments
Water Absorption 0.10 - 0.50 %
0.10 - 0.50 %
24-200 hours
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D >= 90
>= 90
Tensile Strength at Break 49.6 MPa
7200 psi
Elongation at Break 1.8 %
1.8 %
Flexural Strength 60.7 MPa
8800 psi
Compressive Strength 108 MPa
15700 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.586 - 0.669 W/m-K
4.06 - 4.64 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 70.0 °C
158 °F
115 °C
239 °F
Deflection temperature after post-cure
Processing Properties Metric English Comments
Pot Life 30.0 - 45.0 min

@Temperature 25.0 °C
30.0 - 45.0 min

@Temperature 77.0 °F
1-2 lbs
Users viewing this material also viewed the following: