Material Notes:
All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Processing: 100/28 pbw; Potlife: 7-10 h/20°C (68°F), 3-5 h/40°C (105°F), 1-2 h/60°C (140°F); mix at RT; cures in: 20 h/60°C (140°F), 30 min/100°C (212°F), 20 min/140°C (285°F), 1 min + 1-3 h/180°C (356°F).Applications: High temperature performance.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Water Absorption 0.40 - 0.50 %
0.40 - 0.50 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
0.50 - 0.60 %
0.50 - 0.60 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
Viscosity 200 - 300 cP

@Temperature 60.0 °C
200 - 300 cP

@Temperature 140 °F
1000 - 2000 cP

@Temperature 40.0 °C
1000 - 2000 cP

@Temperature 104 °F
20000 - 40000 cP

@Temperature 21.0 °C
20000 - 40000 cP

@Temperature 69.8 °F
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
AboCure
0.00133 bar

@Temperature 180 °C
1.00 torr

@Temperature 356 °F
AboCast
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.95 MPa
10000 psi
Modulus of Elasticity 2.758 GPa
400.0 ksi
Flexural Yield Strength 137.9 MPa
20000 psi
Compressive Yield Strength 124.1 MPa
18000 psi
Thermal Properties Metric English Comments
CTE, linear 60.0 - 70.0 µm/m-°C

@Temperature 20.0 °C
33.3 - 38.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.130 - 0.170 W/m-K
0.902 - 1.18 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 160 °C
320 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.7 - 4.2

@Frequency 1e+6 Hz
3.7 - 4.2

@Frequency 1e+6 Hz
4.0 - 4.5

@Frequency 1000 Hz
4.0 - 4.5

@Frequency 1000 Hz
4.1 - 4.5

@Frequency 50 Hz
4.1 - 4.5

@Frequency 50 Hz
Dielectric Strength 15.7 - 17.7 kV/mm

@Thickness 3.17 mm
400 - 450 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0050 - 0.0070

@Frequency 1000 Hz
0.0050 - 0.0070

@Frequency 1000 Hz
0.020 - 0.040

@Frequency 1e+6 Hz
0.020 - 0.040

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Pot Life 60.0 - 120 min

@Temperature 60.0 °C
60.0 - 120 min

@Temperature 140 °F
180 - 300 min

@Temperature 40.0 °C
180 - 300 min

@Temperature 104 °F
420 - 600 min

@Temperature 20.0 °C
420 - 600 min

@Temperature 68.0 °F