Abatron AboSeal 8104-9 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk

Category Polymer , Adhesive , Thermoset
Manufacturer Abatron
Trade Name AboSeal
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboSeal 8104-9 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboSeal 8104-9 is a 2-part, 100% solids, thixotropic or self-leveling polysulfide. It comes in most colors. It has been made to meet Federal Spec. TT-S-00227-E. It is preferred when white or light colors are needed. It does not stain concrete or marble.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 35 - 40
35 - 40
Tensile Strength at Break 1.03 - 1.38 MPa
150 - 200 psi
Elongation at Break 250 - 300 %
250 - 300 %
Descriptive Properties Value Comments
Color Most Colors
Parts by Weight (pbw) 100
Part A
15
Part B