Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name AboTar
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboTar 8101-8 Solventless Tar-Epoxy Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboTar 8101-8 is a 2-part tar-epoxy variable-ratio system. It is weather- and water-proof, flexible, and acid, alkali, and fuel resistant. It can be used neat or with sand or aggregates. Uses: Resurfacing and reinforcing asphalt surfaces; Resurfacing and weatherproofing wood floors; Consolidating industrial wood-block floors; Pouring new base-surfaces on outdoor decks; Rebuilding ship deck surfaces; Pouring new air-carrier runways on decks; Pouring new commercial and industrial floors. Advantages of AboTar 8101-8: Controllable Flexibility, as in resurfacing asphaltic or bituminous areas with a first soft layer (1 part A/2 parts B, neat or blended with aggregate), followed by harder layers; Non-Critical Ratios, for cases in which proportioning cannot be reliably controlled.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Viscosity <= 1200 cP
<= 1200 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
1/2 Ratio
65
65
1/1 Ratio
75
75
2/1 Ratio
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min

@Temperature 82.222 - 98.889 °C
1.00 - 3.00 hour

@Temperature 180.00 - 210.00 °F
7200 - 10080 min

@Temperature 15.556 - 26.667 °C
120 - 168.0 hour

@Temperature 60.001 - 80.001 °F
(5-7 Days)
Pot Life <= 60 min
<= 60 min
Descriptive Properties Value Comments
Hardening Time (min) 120-720
at ambient temp.; faster with heating
Induction Period (min) >= 15
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved