Material Notes:
Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend allows for visual inspection of proper mixing and ratios. Shelf life: 12+ months (unmixed).Processing: 100/(100-150) ratio. Thixotropic (Vaseline-like consistency) Pot life: 100 g, 8-11 hours at 25°C(77°F). Hardens in 2-4 days at 25°C (77°F), 30-40 min. at 80°C (175°F), 20-25 min. at 120°C (250°F), 15-20 min. at 150°C (300°F).Corrosion Resistance: good resistance to atmospheric conditions, soft and salt water, alkalis and diluted acids.
Physical Properties Metric English Comments
Water Absorption 0.20 %
0.20 %
after 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
100/40 pbw; 68 at 100/80 pbw; 66 (60 after 10 sec) at 100/100 pbw
Tensile Strength, Ultimate 51.0 MPa
7400 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Elongation at Break 3.0 %
3.0 %
Typical averaged test results for Abatron Adhesive/Casting Resins.
Flexural Yield Strength 83.0 MPa
12000 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.
Compressive Yield Strength 115 MPa
16700 psi
Typical averaged test results for Abatron Adhesive/Casting Resins.