Material Notes:
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 93
93
ASTM D785
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 230 %
230 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 1.500 GPa
217.5 ksi
ASTM D638
Flexural Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 5.87 J/cm
11.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F