Aclo Accucomp Polyethylene LD0109L Low Density

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polyethylene LD0109L Low Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.922 g/cc
0.0333 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
MD; ASTM D955
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 40
40
ASTM D785
Tensile Strength at Break 8.00 MPa
1160 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 112 %
112 %
ASTM D638
Elongation at Yield 27 %
27 %
ASTM D638
Tensile Modulus 0.320 GPa
46.4 ksi
ASTM D638
Flexural Strength 9.03 MPa
1310 psi
ASTM D790
Flexural Modulus 0.300 GPa
43.5 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 °C
113 °F
ASTM D648