Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp Polypropylene CPO402V Automotive Approved Copolymer Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
MD; ASTM D955
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 62
62
ASTM D785
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Tensile Modulus 0.680 GPa
98.6 ksi
ASTM D638
Flexural Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 0.680 GPa
98.6 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.2 °C
144 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 47.8 °C
118 °F