Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Aclo Compounders
Trade Name Accuguard
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
MD; ASTM D955
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Tensile Modulus 0.800 GPa
116 ksi
ASTM D638
Flexural Strength 27.6 MPa
4000 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °C
113 °F
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
UL File #99379(N)
Copyright © lookpolymers.com All Rights Reserved