Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene CP0435G43CV Copolymer Glass Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene CP0435G43CV Copolymer Glass Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Approved to GMP.PP.039 Black A13054
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Tensile Modulus 5.00 GPa
725 ksi
ASTM D638
Flexural Strength 80.0 MPa
11600 psi
ASTM D790
Flexural Modulus 6.498 GPa
942.5 ksi
ASTM D790
Izod Impact, Notched 2.62 J/cm
4.90 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 162 °C
324 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Users viewing this material also viewed the following: