Aclo Accutech Polypropylene Copolymer CP0436W30L1 Wollastonite Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436W30L1 Wollastonite Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 30 %
30 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 50
50
ASTM D785
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.350 GPa
340.8 ksi
ASTM D638
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Flexural Modulus 2.150 GPa
311.8 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm
1.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 109 °C
228 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C
144 °F