Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.20 - 2.23 g/cc
2.20 - 2.23 g/cc
ASTM D792
Deformation 5.4 - 6.4 %
5.4 - 6.4 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
10 - 12 %
10 - 12 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 56 - 60
56 - 60
ASTM D2240
Ball Indentation Hardness 44.0 - 48.0 MPa
6380 - 6960 psi
ISO 2032-N132
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
ASTM D4894
Elongation at Break >= 210 %
>= 210 %
ASTM D4894
Coefficient of Friction, Dynamic 0.11 - 0.13
0.11 - 0.13
ASTM D1894
Coefficient of Friction, Static 0.18 - 0.20
0.18 - 0.20
ASTM D1894
Thermal Properties Metric English Comments
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -120 °C
-184 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Users viewing this material also viewed the following: