Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.01 - 2.03 g/cc
2.01 - 2.03 g/cc
ASTM D792
Deformation 2.0 - 4.5 %
2.0 - 4.5 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 51 - 56
51 - 56
ASTM D2240
Ball Indentation Hardness 100 - 120 MPa
14500 - 17400 psi
ISO 2032-N132
Tensile Strength at Break >= 10.0 MPa
>= 1450 psi
ASTM D4745-11
Elongation at Break >= 130 %
>= 130 %
ASTM D4745-11
Coefficient of Friction, Static 0.10 - 0.30
0.10 - 0.30
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 335 °C
635 °F
DSC
Maximum Service Temperature, Air 250 °C
482 °F
DSC
Minimum Service Temperature, Air -100 °C
-148 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
ASTM D257
Dielectric Strength 12.0 - 20.0 kV/mm
305 - 508 kV/in
ASTM D149