Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Adamas
Trade Name Adalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 814 PTFE, 55% Bronze, 5% MoS2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 3.81 - 3.83 g/cc
3.81 - 3.83 g/cc
ASTM D792
Deformation 2.0 - 3.0 %
2.0 - 3.0 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
4.0 - 6.0 %
4.0 - 6.0 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 63
60 - 63
ASTM D2240
Ball Indentation Hardness 57.0 - 60.0 MPa
8270 - 8700 psi
ISO 2032-N132
Tensile Strength at Break >= 12.0 MPa
>= 1740 psi
ASTM D4894
Elongation at Break >= 80 %
>= 80 %
ASTM D4894
Coefficient of Friction, Dynamic 0.16 - 0.18
0.16 - 0.18
ASTM D1894
Coefficient of Friction, Static 0.18 - 0.20
0.18 - 0.20
ASTM D1894
Thermal Properties Metric English Comments
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -100 °C
-148 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm
1.00e+7 ohm-cm
ASTM D257
Users viewing this material also viewed the following: