Adamas Adalon® 992 Modified PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Adamas
Trade Name Adalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 992 Modified PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.15 - 2.17 g/cc
2.15 - 2.17 g/cc
ASTM D792
Deformation 5.0 - 6.4 %
5.0 - 6.4 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
9.0 - 10.8 %
9.0 - 10.8 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 52 - 58
52 - 58
ASTM D2240
Ball Indentation Hardness 60.0 - 64.0 MPa
8700 - 9280 psi
ISO 2032-N132
Tensile Strength at Break >= 30.0 MPa
>= 4350 psi
ASTM D4745-11
Elongation at Break >= 420 %
>= 420 %
ASTM D4745-11
Coefficient of Friction, Dynamic 0.080 - 0.10
0.080 - 0.10
ASTM D1894
Coefficient of Friction, Static 0.10 - 0.13
0.10 - 0.13
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -160 °C
-256 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Dielectric Strength 60.0 - 80.0 kV/mm
1520 - 2030 kV/in
ASTM D149