Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addcomp ADD-VANCE® SA 155 Slip Masterbatch, PP homopolymer base

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® SA 155 Slip Masterbatch, PP homopolymer base.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Improves slip properties of Polyolefins. Also it can be used as a release agent for injection molded productsExamples: (L)LDPE, HDPE, and PP films, sheets, profiles, injection molded products, etc.Mode of action and advantages: ADD-VANCE SA 155 provides excellent slip properties. ADD-VANCE SA 155 reduces friction between two surfaces for instance between polymer and metal. As a consequence the slip properties of the product are improvedAdvantages: Highly effective, very long lasting slip properties, already at low dosing rates; Excellent organoleptic properties; Good printability; Non-toxic, non-corrosive and thermally stable (>250 °C); Injection molding: also improved demolding and product release; Non-sticking pellets, dust free; and Safe and easy handlingRegulations: ADD-VANCE SA 155 complies with the directive 2002/72/EEC for food approval. The active ingredient in ADD-VANCE SA 155 complies with FDA 21 CFR § 177.1520 Olefin polymers.Information provided by ADDCOMP
Processing Properties Metric English Comments
Processing Temperature <= 250 °C
<= 482 °F
Descriptive Properties Value Comments
Appearance Slightly yellow granules
Dosing Level 0.2-2.0%