Addiplast Addilene J 470 ST14 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Addiplast
Trade Name Addilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene J 470 ST14 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Soft touchInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183/A
Melt Flow 17 g/10 min
17 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ISO 868
Tensile Strength at Break 11.0 MPa
1600 psi
ISO R 527
Tensile Strength, Yield 15.0 MPa
2180 psi
ISO R 527
Elongation at Yield 50 %
50 %
ISO R 527
Modulus of Elasticity 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ISO 75-2/AF
Vicat Softening Point 143 °C
289 °F
ISO 306/A50
Electrical Properties Metric English Comments
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A