Material Notes:
Unreinforced, medium viscosityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
Conditioned; ISO 868
84
84
ISO 868
Tensile Strength, Yield 85.0 MPa
12300 psi
ISO R 527
90.0 MPa
13100 psi
Conditioned; ISO R 527
Elongation at Yield 40 %
40 %
ISO R 527
>= 50 %
>= 50 %
Conditioned; ISO R 527
Modulus of Elasticity 1.20 GPa
174 ksi
Conditioned; ISO 178
2.80 GPa
406 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180/1A
12.0 kJ/m²
5.71 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
NB
NB
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/IeA
1.10 J/cm²
5.23 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM E831
Melting Point 260 °C
500 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Conditioned; CEI 60093
1.00e+15 ohm
1.00e+15 ohm
CEI 60093
Dielectric Strength 27.0 kV/mm
686 kV/in
Conditioned; CEI 60243-1
28.0 kV/mm
711 kV/in
CEI 60243-1
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A