Material Notes:
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Conditioned; ISO 868
86
86
ISO 868
Tensile Strength at Break 160 MPa
23200 psi
Conditioned; ISO R 527
210 MPa
30500 psi
ISO R 527
Elongation at Yield 2.0 %
2.0 %
ISO R 527
4.0 %
4.0 %
Conditioned; ISO R 527
Modulus of Elasticity 7.70 GPa
1120 ksi
Conditioned; ISO 178
10.5 GPa
1520 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1A
17.0 kJ/m²
8.09 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179/IeU
7.50 J/cm²
35.7 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179/IeA
1.60 J/cm²
7.61 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM E831
Melting Point 260 °C
500 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 255 °C
491 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1
35.0 kV/mm
889 kV/in
CEI 60243-1
Comparative Tracking Index 600 V
600 V
CEI 60112/Solution A