Addiplast Addinyl B2 1 Flame Retardant Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant
Manufacturer Addiplast
Trade Name Addinyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl B2 1 Flame Retardant Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, halogen freeInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
Conditioned; ISO 868
82
82
ISO 868
Tensile Strength at Break 40.0 MPa
5800 psi
Conditioned; ISO R 527
50.0 MPa
7250 psi
ISO R 527
Elongation at Break 3.0 %
3.0 %
ISO R 527
15 %
15 %
Conditioned; ISO R 527
Modulus of Elasticity 1.90 GPa
276 ksi
Conditioned; ISO 178
3.30 GPa
479 ksi
ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
ISO 180/1A
8.00 kJ/m²
3.81 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
ISO 179/IeA
0.700 J/cm²
3.33 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75-2/AF
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Oxygen Index 37 %
37 %
ISO 4589
Glow Wire Test 960 °C
1760 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Conditioned; CEI 60093
1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Dielectric Strength 26.0 kV/mm
660 kV/in
CEI 60243-1
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A