Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 10% Glass Fiber Reinforced , Nylon 66/6, Mineral Reinforced
Manufacturer Addiplast
Trade Name Addinyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Conditioned; ISO 868
84
84
ISO 868
Tensile Strength at Break 60.0 MPa
8700 psi
Conditioned; ISO R 527
105 MPa
15200 psi
ISO R 527
Elongation at Yield 5.0 %
5.0 %
ISO R 527
9.0 %
9.0 %
Conditioned; ISO R 527
Modulus of Elasticity 3.50 GPa
508 ksi
Conditioned; ISO 178
7.50 GPa
1090 ksi
ISO 178
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO 180/1A
7.00 kJ/m²
3.33 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/IeU
6.00 J/cm²
28.6 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179/IeA
0.700 J/cm²
3.33 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E831
Melting Point 243 °C
469 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
428 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Comparative Tracking Index 600 V
600 V