Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell AI-30 Nylon 66, Impact Modified

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Adell Plastics, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell AI-30 Nylon 66, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0125 cm/cm
0.0125 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Ultimate 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Compressive Yield Strength 76.0 MPa
11000 psi
ASTM D695
Izod Impact, Notched 1.70 J/cm
3.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
351 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: