Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Adell RR-39 Polypropylene Copolymer; 43% Glass Reinforced, High Impact

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass Reinforced, Impact Modified
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell RR-39 Polypropylene Copolymer; 43% Glass Reinforced, High Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Adell Plastics, Inc.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 63.0 MPa
9140 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 105 MPa
15200 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
1.30 J/cm

@Temperature -40.0 °C
2.44 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Izod Impact, Unnotched 5.30 J/cm
9.93 ft-lb/in
ASTM D256
4.80 J/cm

@Temperature -40.0 °C
8.99 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Gardner Impact 1.10 J
0.811 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
ASTM D648
Users viewing this material also viewed the following: