Adell WR-37 33% Glass Reinforced PET

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced
Manufacturer Adell Plastics, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adell WR-37 33% Glass Reinforced PET.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
24 hr immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 112
112
ASTM D785
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 160 MPa
23200 psi
ASTM D638
Flexural Strength 240 MPa
34800 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Yield Strength 233 MPa
33800 psi
ASTM D695
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 232 - 249 °C
450 - 480 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 247 °C
477 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Flammability, UL94 HB
HB