Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.Features: High flowGood surface appearance on molded partsGood tensile propertiesGood tear strengthProduct Notes: Values are for injection molded plaques, side gated.82.6 mm x 117.5 mm x 3 mmInformation provided by Advanced Elastomer Systems.Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Melt Flow 49 g/10 min

@Load 5.00 kg,
Temperature 230 °C
49 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
5 seconds; ASTM D2240
Tensile Strength at Break 7.52 MPa
1090 psi
Across flow; ASTM D412
Tensile Strength, Yield 4.80 MPa
696 psi
At 100% elongation, across flow; ASTM D412
Elongation at Break 740 %
740 %
Across flow; ASTM D412
Tensile Modulus 0.100 GPa
14.5 ksi
1mm/min; DIN 53457
Flexural Modulus 0.0990 GPa
14.4 ksi
1.7 mm/min; DIN 53457
Izod Impact, Notched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 180A
Tear Strength 54.3 kN/m
310 pli
73°F; ASTM D624
Compression Set 41 %
41 %
73°F, 22 hr, Method B; ASTM D395
57 %
57 %
158°F, 22 hr, Method B; ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 55.0 °C
131 °F
Vicat A, 1 kg; DIN 53460/ISO 306
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 175 - 240 °C
347 - 464 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F