Material Notes:
The 2100 Series grades of Alcryn® offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn®. The new 2100 grades bond to polycarbonate, ABS, polycarbonate/ABS alloys, SAN, ASA, copolyester elastomers and TPUs, as well as both flexible and rigid PVC. The 2100 seriesis high flow in general plastic processingis designed for injection molding and overmoldingis excellent for complex extrusionsis excellent for co-extrusionsinjection molded and overmolded partssoft touch handles and grips on appliance and tool applicationsautomotive interior applicationsnoise and vibration deadeningseals and gaskets for automotive insert moldingwindow and door weather stripping (and other complex profile extrusions)coated fabrics and sheet goodswire and cable jacketstubing and hoseblow molded partsInformation provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D471
Viscosity 232000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
232000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
After 7 days at 125°C; ASTM D573
66
66
ASTM D2240
Tensile Strength at Break 11.71 MPa
1698 psi
After 7 days at 125°C; ASTM D573
12.20 MPa
1769 psi
ASTM D412
Elongation at Break 518.7 %
518.7 %
After 7 days at 125°C; ASTM D573
570 %
570 %
ASTM D412
100% Modulus 0.00310 GPa
0.450 ksi
ASTM D412
0.003382 GPa
0.4905 ksi
After 7 days at 125°C; ASTM D573
Graves Tear Strength 46.02 kN/m

@Temperature 24.0 °C
262.5 pli

@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 34 %
34 %
After 22 Hr At 24°C; ASTM D395
83 %
83 %
After 22 Hr at 100°C; ASTM D395
Tensile Set 13 %
13 %
ASTM D412
Processing Properties Metric English Comments
Processing Temperature 177 °C
351 °F
Descriptive Properties Value Comments
Fluid Resistance - Volume Change, % (ASTM D471) -16
After 7 Days in ASTM Oil No. 1 At 212°F (100°C)
19
After 7 Days in ASTM Ref. Fuel no. B at 75°F (24°C)
7
After 7 Days in Water at 212°F (100°C)
9
After 7 Days in IRM 903 Oil No. 3 at 212°F (100°C)
Users viewing this material also viewed the following: