Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE features excellent soft touch feel, will bond to ABS, PC, Isoplast, clear copolyester and acrylics, and because it is translucent it is easily colored with a minimum of concentrate. DuraGrip® TPE is not hygroscopic and under normal conditions does not require drying.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D471; ISO 2781
Viscosity 302000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
302000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
Time of 5 seconds; ASTM D2240; ISO 48
Tensile Strength, Ultimate 8.929 MPa
1295 psi
ASTM D412; ISO 37
Elongation at Break 644 %
644 %
ASTM D412; ISO 37
100% Modulus 0.00120 GPa
0.174 ksi
ASTM D412; ISO 37
Processing Properties Metric English Comments
Processing Temperature 216 °C
420 °F