Advanced Polymer Alloys DuraGrip™ DGR 6150 NC Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer APA - Advanced Polymer Alloys
Trade Name DuraGrip™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys DuraGrip™ DGR 6150 NC Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraGrip® DGR 6150 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylon, ASA, PC/ABS alloys, PBT, and PC/PBT alloys. It is easy to use in injection molding and extrusion processes. DGR 6150NC has excellent elastomeric properties and soft touch feel. DuraGrip® bonding grades are hygroscopic, and for best results drying is recommended prior to use.Information provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D471
Viscosity 327000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
327000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 52
52
5 Sec; ASTM D2240
Tensile Strength at Break 5.90 MPa
855 psi
ASTM D412
Elongation at Break 360 %
360 %
ASTM D412
100% Modulus 0.00180 GPa
0.261 ksi
ASTM D412
Graves Tear Strength 29.8 kN/m

@Temperature 24.0 °C
170 pli

@Temperature 75.2 °F
Die C; ASTM D624
Compression Set 19 %
19 %
after 22 Hr At 24°C; ASTM D395
Tensile Set 3.0 %
3.0 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -68.0 °C
-90.4 °F
ASTM D746
Descriptive Properties Value Comments
Color N,B
Users viewing this material also viewed the following: