Aearo E-A-R Specialty Composites Isoloss® VL Polyurethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Aearo E-A-R Specialty Composites
Trade Name Isoloss®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aearo E-A-R Specialty Composites Isoloss® VL Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isoloss® VL elastomers have an extremely low modulus and good damping performance throughout a useful range of 0°C to 49°C. Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protection for sensitive mechanisms within minimum sway parameters, and quick return to equilibrium after vibrations or shocks.Information provided by Aearo E-A-R Specialty Composites.
Mechanical Properties Metric English Comments
Hardness, Shore A 24
24
Tensile Strength at Break 1.77 MPa
256 psi
Elongation at Break 900 %
900 %
Resilience 23
23
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Brittleness Temperature -40.0 °C
-40.0 °F
Flammability, UL94 V-0
V-0
Descriptive Properties Value Comments
Abrasion Resistance Good
Compression Set Resistance Good to Excellent
Damping T max 6 dB
Heat Aging; 100°C Excellent
Tear Strength Excellent