Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatures as well as easy processing. AKROMID® A is an engineering plastic compound that allows a broad range of possible applications. On the basis of these standard types, we are able to develop individual compounds for special application needs.Information from Akro-Plastic
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183
Filler Content 50 %
50 %
ISO 1172
Water Absorption 1.3 - 1.5 %

@Temperature 70.0 °C
1.3 - 1.5 %

@Temperature 158 °F
62% r.h., Humidity; ISO 62
Water Absorption at Saturation 3.7 - 4.3 %

@Time 82800 sec
3.7 - 4.3 %

@Time 23.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0025 cm/cm
0.0025 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
5 [mm/min]; ISO 527-1/2
Elongation at Break 3.5 %
3.5 %
5 [mm/min]; ISO 527-1/2
Tensile Modulus 12.6 GPa
1830 ksi
1[mm/min]; ISO 527-1/2
Flexural Strength 310 MPa
45000 psi
2 [mm/min]; ISO 178
Flexural Modulus 13.6 GPa
1970 ksi
2 [mm/min]; ISO 178
Charpy Impact Unnotched 11.0 J/cm²

@Temperature 23.0 °C
52.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.30 J/cm²

@Temperature 23.0 °C
10.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
ISO 11357-1/3
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093