Albis Plastics ASA 02A MR20 , 20% Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , ASA Polymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics ASA 02A MR20 , 20% Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Melt Temperature: 465-535°F, Mold Temperature: 105-175°F)Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Melt Flow 13.9 g/10 min
13.9 g/10 min
220C/10,000 g; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Tensile Strength, Yield 37.2 MPa
5400 psi
ASTM D638
Flexural Yield Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C
183 °F
ASTM D648
Vicat Softening Point 101 °C
214 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 241 - 279 °C
466 - 534 °F
Injection
Mold Temperature 41.0 - 79.0 °C
106 - 174 °F