Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Clutch Components, BushingsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Elongation at Break 2.5 %
2.5 %
DIN 53 455
Flexural Yield Strength 230 MPa
33400 psi
DIN 53 452
Flexural Modulus 13.5 GPa
1960 ksi
DIN 53 457
Izod Impact, Notched 1.98 J/cm
3.71 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Electrical Properties Metric English Comments
Surface Resistance <= 200 ohm
<= 200 ohm
DIN 53 482
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F