Material Notes:
105°C rated insulation compound
Mechanical Properties Metric English Comments
Tensile Strength 20.0 MPa
2900 psi
Elongation at Break 230 %
230 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -12.0 °C
10.4 °F
Oxygen Index 27 %
27 %