Category | Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade |
Manufacturer | AlphaGary |
Trade Name | SuperKleen |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | AlphaGary SuperKleen SK/3003-85 CLEAR 0003 Flexible Polyvinyl Chloride Compound.pdf |
Price | EMAIL US sales@lookpolymers.com |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 45 - 95 | 45 - 95 | |
85 | 85 | Typical |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Transmission, Visible | 90 % | 90 % | Clear; thickness not specified |
Descriptive Properties | Value | Comments |
---|---|---|
DEHP Free | Yes | |
Phthalate Free | Yes |