  Online Service   lookpolymers   27660005
Material Notes:
PP HOMO 011 features high molecular weight, high isotactic, and does not contain slip or anti-block. Applications include strapping, various extrusion profile, and sheet and film applications.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Index of Compound 1.1 g/10 min

@Temperature 230 °C
1.1 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 33.1 MPa
4800 psi
50 mm/min; ASTM D638
Elongation at Break >= 10 %
>= 10 %
50 mm/min; ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Temperature 22.8 °C
0.900 ft-lb/in

@Temperature 73.0 °F
ASTM D256