Material Notes:
PP HOMO 038X features low water carryover. Applications include woven fabric and bags, rope and cordage, woven carpet backing, and woven geotextile fabrics.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Index of Compound 3.8 g/10 min

@Temperature 230 °C
3.8 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Hardness, Shore D 71
71
ASTM D2240
Tensile Strength, Yield 36.9 MPa
5350 psi
50 mm/min; ASTM D638
Flexural Modulus 1.59 GPa
230 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature 22.8 °C
0.700 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648