American Elements C-MITE™ Cerium Oxide Nanopowder

Category Ceramic , Oxide
Manufacturer American Elements
Trade Name C-MITE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements C-MITE™ Cerium Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionApplicationsC-MITE™ powders and dispersions recently developed are inorganic cerium-oxide nanoparticles with unique polishing and Ultra-Violet attenuating properties. C-MITE-A™ products are uncoated and hydrophilic. C-MITE-O™ products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm.
Physical Properties Metric English Comments
Density 7.65 g/cc
0.276 lb/in³
Molecular Weight 172.12 g/mol
172.12 g/mol
Thermal Properties Metric English Comments
Melting Point 2400 °C
4350 °F
Descriptive Properties Value Comments
Appearance Brown to Yellow
Solubility Soluble in water and strong mineral acids