American Elements Carbon Nanoparticles

Category Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Carbon Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionCarbon (C) Nanoparticles, nanodots or nanopowder are black spherical high surface area graphitic carbon. Nanoscale Carbon Particles are typically 10 - 45 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 75 - 100 nm range with a specific surface area of approximately 2 - 10 m 2 /g. Nano Carbon Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms.
Physical Properties Metric English Comments
Particle Size 0.010 - 0.045 µm
0.010 - 0.045 µm
0.075 - 0.10 µm
0.075 - 0.10 µm
Specific Surface Area 2.0 - 10 m²/g
2.0 - 10 m²/g
30 - 50 m²/g
30 - 50 m²/g
Descriptive Properties Value Comments
Appearance Black