American Elements Gold Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Gold Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionGold (Au) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Gold Particles are typically 20 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 3 m 2 /g range. Nano Gold Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for gold nanocrystals include as an anti-microbial, anti-biotic and anti-fungal agent when incorporated in coatings, plastics, nanofiber and textiles and in nanowire and certain catalyst applications. Coat gold particles with DNA and inject them into plant cells or plant embryos. Some genetic material will remain in the cells and transform them. This method allows transformation of plant plastids. The transformation efficiency is lower than in agro bacterial mediated transformation.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.10 µm
0.020 - 0.10 µm
Specific Surface Area 1.0 - 3.0 m²/g
1.0 - 3.0 m²/g
Molecular Weight 196.97 g/mol
196.97 g/mol
Descriptive Properties Value Comments
Appearance Brown