American Elements Iridium Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Iridium Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionIridium (Ir) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Iridium Particles are typically 20 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 5 m 2 /g range. Nano Iridium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Iridium nanocrystals include numerous uses in catalysts, electrocatalysts, chemical synthesis, biphasic catalysis and hydrogenation reactions, and as a Magnetic Nanopowder, in polymer membranes to create Active Polymer Membranes and in other coatings, plastics, nanofiber and textiles and in nanowire and other catalysis applications.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.10 µm
0.020 - 0.10 µm
Specific Surface Area 1.0 - 5.0 m²/g
1.0 - 5.0 m²/g
Molecular Weight 192.22 g/mol
192.22 g/mol
Descriptive Properties Value Comments
Appearance Black