Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Elements Manganese Nanoparticles

Category Metal , Nonferrous Metal , Pure Element
Manufacturer American Elements
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements Manganese Nanoparticles.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionManganese (Mn) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Manganese Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 30 – 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7 m 2 /g. Nano Manganese Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Manganese Nanocrystals include as a Magnetic Nanoparticle (also in iron-manganese nanoparticles) for magnetic data storage and magnetic resonance imaging (MRI), in biosensors and in coatings, plastics, nanowire, nanofiber and textiles and in certain alloy and catalyst applications. Further research is being done for their potential electrical, optical, imaging, biomedical and bioscience properties. Manganese Nano Particles are generally immediately available in most volumes.
Physical Properties Metric English Comments
Particle Size 0.020 - 0.040 µm
0.020 - 0.040 µm
0.10 µm
0.10 µm
Specific Surface Area 7.0 m²/g
7.0 m²/g
30 - 50 m²/g
30 - 50 m²/g
Molecular Weight 54.94 g/mol
54.94 g/mol
Descriptive Properties Value Comments
Appearance Silvery
Users viewing this material also viewed the following: