Material Notes:
General DescriptionSilicon (Si) Nanoparticles, nanodots or Nanopowder are spherical high surface area metal particles. Nanoscale Silicon Particles are typically 5-25 nanometers (nm) with specific surface area (SSA) in the 30 – 70 m 2 /g range and also available with an average particle size of 80 -100 nm range with a specific surface area of approximately 5 - 10 m 2 /g. Nano Silicon Particles are also available in ultra high purity and high purity and carbon coated and dispersed forms. Applications for silicon nanocrystals include in luminescent display devises due to their broader excitation spectra, as building blocks for single-nanoparticle electronic devices, in micro and integrated semiconductors, in solar energy cells, for production of silicon nanotubes and in nanowire, nanofiber and in certain alloy applications. Further research is being done for their potential electrical, optical, imaging, and bioscience properties.
Physical Properties Metric English Comments
Density 2.33 g/cc
0.0842 lb/in³
Particle Size 0.0050 - 0.025 µm
0.0050 - 0.025 µm
0.080 - 0.10 µm
0.080 - 0.10 µm
Specific Surface Area 5.0 - 10 m²/g
5.0 - 10 m²/g
30 - 70 m²/g
30 - 70 m²/g
Molecular Weight 28.08 g/mol
28.08 g/mol
Thermal Properties Metric English Comments
Melting Point 1414 °C
2577 °F
Boiling Point 2900 °C
5250 °F
Descriptive Properties Value Comments
Appearance Silvery