American Elements T-MITE™ Titanium Oxide Nanopowder

Category Ceramic , Oxide , Titanium Oxide
Manufacturer American Elements
Trade Name T-MITE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Elements T-MITE™ Titanium Oxide Nanopowder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionT-MITE™ powders and dispersions are recently developed inorganic titanium dioxide nanoparticles which impart special UV filtering and reflective properties to coatings and surfaces. T-MITE-A™ products are uncoated and hydrophilic. T-MITE-O™ products are coated with an organic silane (1-4%) and are hydrophobic. Particles are available in the size range of 10-200 nm.
Physical Properties Metric English Comments
Density 4.23 g/cc
0.153 lb/in³
Molecular Weight 79.9 g/mol
79.9 g/mol
Thermal Properties Metric English Comments
Melting Point 1800 °C
3270 °F
Descriptive Properties Value Comments
Appearance White